Co
CO5093
Cobalt Wire
- Diameter:
- 1 mm
- Purity:
- 99.998+%
- Description:
- Temper annealed. Electron Beam melted. under Argon.
Technical Data:
POA = Price on application. Batch Gi4924 Mechanical test data : Yield Strength 74412 MPa. Ultimate Tensile Strength 1073.46 MPa.... POA = Price on application. Batch Gi4924 Mechanical test data : Yield Strength 74412 MPa. Ultimate Tensile Strength 1073.46 MPa. Elongation in 8 In %: 20 Actual analysis Gi4924 ppm: Ag <0.01, Al 0.09, As<0.1, Au<0.05, B<0.001, Ba<0.005, Be<0.001, Bi<0.001, .....................Nd<0.005, Ni 2.8, O 164, Os<0.001, P 1.2, Pb<0.01, Pd<0.01, Pt<0.05,Rb<0.005, Re 0.01, Rh<0.005, Ru<0.01, S 1, Sb<0.05, Sc<0.001, Se<0.02, Si 0.21, Sn<0.05, Sr<0.001, Ta<1, Te<0.05, Th<0.0001, Ti<0.01, Tl<0.005, U<0.0001, V 0.03, W<0.01, Y<0.001, Zn<0.1, Zr<0.01. Total impurities 182.9992