Zr
ZR2457
Zirconium Plate
- Thickness:
- 7.0 mm
- Purity:
- 97.0%
- Description:
- Temper annealed pickled.
Technical Data:
Hazards - flammable solid. Tolerance on width - length -0.0mm +2mm. POA = Price on application. ASTM B551 Grade 2 R60702... Hazards - flammable solid. Tolerance on width - length -0.0mm +2mm. POA = Price on application. ASTM B551 Grade 2 R60702 Zirconium Plate 702, ASME SB 551, BP-M10, EN 10204 3.1. Specification analysis maz ppm: Zr+Hf 99.2% min, Hf 4.6%, max, Fe+Cr<=2000, H<=50, C<=600, O<=1600. Ingot analysis typical Zr+Hf >=99.2%, Hf 1.1%, Fe+Cr 1600, H 10, N 80, C200, O 1600.